Refractory Technology Upper portion of hot metal mixer are lined with mullite bricks, which helps in resisting the Neither A nor B Corrosion by layer of slag Washing action of metal Both A & B Neither A nor B Corrosion by layer of slag Washing action of metal Both A & B ANSWER DOWNLOAD EXAMIANS APP
Refractory Technology Outer combustion chamber of blast furnace stove is lined with __________ bricks. Zirconia Fireclay Silica Chrome magnesite Zirconia Fireclay Silica Chrome magnesite ANSWER DOWNLOAD EXAMIANS APP
Refractory Technology Thermal conductivity of refractory bricks Decreases with decreases in porosity Increases with the amount of air entrapped in pores Increases with decrease in porosity Is independent of its porosity and is maximum for insulating bricks Decreases with decreases in porosity Increases with the amount of air entrapped in pores Increases with decrease in porosity Is independent of its porosity and is maximum for insulating bricks ANSWER DOWNLOAD EXAMIANS APP
Refractory Technology Rate of slag attack on refractories increases with rise in temperature due to the None of these Oxidising condition in the furnace Increased thermal conductivity of brick Decreased viscosity of slag None of these Oxidising condition in the furnace Increased thermal conductivity of brick Decreased viscosity of slag ANSWER DOWNLOAD EXAMIANS APP
Refractory Technology Maximum apparent porosity of magnesite bricks is about __________ percent. 24 8 58 44 24 8 58 44 ANSWER DOWNLOAD EXAMIANS APP
Refractory Technology Spalling tendency of refractories is reduced by increasing its Thermal conductivity Porosity Strength Specific gravity Thermal conductivity Porosity Strength Specific gravity ANSWER DOWNLOAD EXAMIANS APP