Materials and Construction Nickel (56%) and molybdenum (17%) alloys are called Monel Hastealloy C Bronzes Inconel Monel Hastealloy C Bronzes Inconel ANSWER DOWNLOAD EXAMIANS APP
Materials and Construction Polythene (low or high density) containers are not corroded by Sulphur trioxide at 60°C Any of these Sulphuric acid (10%) at room temperature Nitric acid (95%) at room temperature Sulphur trioxide at 60°C Any of these Sulphuric acid (10%) at room temperature Nitric acid (95%) at room temperature ANSWER DOWNLOAD EXAMIANS APP
Materials and Construction The most distinguished property of malleable cast iron is its high Hardness Malleability None of these Ductility Hardness Malleability None of these Ductility ANSWER DOWNLOAD EXAMIANS APP
Materials and Construction Slow and progressive deformation of a material with time under constant stress is called Creep None of these Erosion Resilience Creep None of these Erosion Resilience ANSWER DOWNLOAD EXAMIANS APP
Materials and Construction Addition of __________ to the steel helps in increasing the residual magnetism in steel used for making magnets. Cobalt Tungsten Nickel Chromium Cobalt Tungsten Nickel Chromium ANSWER DOWNLOAD EXAMIANS APP
Materials and Construction Which of the following has the poorest wel-dability? Wrought iron High-carbon steel Low carbon steel Mild steel Wrought iron High-carbon steel Low carbon steel Mild steel ANSWER DOWNLOAD EXAMIANS APP