Manufacturing And Production Technology Crater wear leads to Increase in cutting temperature Weakening of tool All of these Friction and cutting forces Increase in cutting temperature Weakening of tool All of these Friction and cutting forces ANSWER DOWNLOAD EXAMIANS APP
Manufacturing And Production Technology Stellite preserves hardness up to a temperature of 350°C 1100°C 500°C 900°C 350°C 1100°C 500°C 900°C ANSWER DOWNLOAD EXAMIANS APP
Manufacturing And Production Technology A right hand tool on a lathe cuts most efficiently when it travels From left to right end of the lathe bed Across the bed From right to left end of the lathe bed With the help of a compound slide From left to right end of the lathe bed Across the bed From right to left end of the lathe bed With the help of a compound slide ANSWER DOWNLOAD EXAMIANS APP
Manufacturing And Production Technology The size of a lathe is specified by the All of these Swing diameter over the carriage Length between centers Swing diameter over the bed All of these Swing diameter over the carriage Length between centers Swing diameter over the bed ANSWER DOWNLOAD EXAMIANS APP
Manufacturing And Production Technology Tool life is generally better when Hard constituents are present in the micro-structure of the tool material Grain size of the metal is small Grain size of the metal is large None of the listed here Hard constituents are present in the micro-structure of the tool material Grain size of the metal is small Grain size of the metal is large None of the listed here ANSWER DOWNLOAD EXAMIANS APP
Manufacturing And Production Technology The cutting speed for drilling aluminium, brass and bronze with carbon steel drills is ___ cutting speed for drilling mild steel with high speed steel drills. None of the listed here More than Less than Equal to None of the listed here More than Less than Equal to ANSWER DOWNLOAD EXAMIANS APP