Chemical Engineering Basics Castability of aluminium is increased by the addition of __________ in it. Bismuth Lead Silicon Manganese Bismuth Lead Silicon Manganese ANSWER DOWNLOAD EXAMIANS APP
Chemical Engineering Basics Brinell Hardness Number (BHN) for talc is approximately in the range of 200-250 1-5 100-150 20-30 200-250 1-5 100-150 20-30 ANSWER DOWNLOAD EXAMIANS APP
Chemical Engineering Basics Powder metallurgy is used to produce High precision components with complex cavities and sharp features Porosity free components Components of large size Components of such alloys whose constituents do not form alloys readily High precision components with complex cavities and sharp features Porosity free components Components of large size Components of such alloys whose constituents do not form alloys readily ANSWER DOWNLOAD EXAMIANS APP
Chemical Engineering Basics Oxygen cylinders used for autogenous (cutting/welding) purposes are Heat treated before use Made by sand casting Seamless & made of steel Welded steel cylinders Heat treated before use Made by sand casting Seamless & made of steel Welded steel cylinders ANSWER DOWNLOAD EXAMIANS APP
Chemical Engineering Basics __________ test can be termed as the semi-distructive test. Torsion Hardness Charpy Impact Torsion Hardness Charpy Impact ANSWER DOWNLOAD EXAMIANS APP
Chemical Engineering Basics Blast furnace slag is mainly molten Magnesium silicate Sand Calcium silicate Iron pyrite Magnesium silicate Sand Calcium silicate Iron pyrite ANSWER DOWNLOAD EXAMIANS APP